7075-T6

The alloy 7075-T6 is a high-strength 7000 series aluminum alloy of zinc, magnesium and copper, heat treated and aged to the T6 temper.

Every 7075-T6 article of the Metal CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

The alloy 7075-T6 is a high-strength 7000 series aluminum alloy of zinc, magnesium and copper, heat treated and aged to the T6 temper. The Aluminum Association limits on ASM’s sheet are 5.1 to 6.1 % zinc, 2.1 to 2.9 % magnesium and 1.2 to 2.0 % copper. Its copper and zinc buy the strength. ASM lists aircraft fittings, gears and shafts, worm gears and defense parts among its uses.

Datasheet Figures

ASM prints a typical ultimate tensile strength of 572 MPa (83,000 psi) and a yield strength of 503 MPa (73,000 psi). Brinell hardness is 150 and shear strength 331 MPa (48,000 psi). Fatigue strength at 500 million cycles is 159 MPa (23,000 psi). The modulus of 71.7 GPa (10,400 ksi) is only 4 % above that of 6061-T6. The machinability rating is 70 on ASM’s scale of aluminum alloys.
Read More

Direction and Toughness

Elongation stays at 11 % in both sheet and bar. ASM gives fracture toughness of 20, 25 and 29 MPa·m½ (18.2, 22.8 and 26.4 ksi·in½) in three directions. The best direction equals the single figure for 6061-T6, and the weakest is a third lower. A sharp internal corner or a cross hole in 7075 has less room to spread a local overload.

Temper Options

For T6, the alloy is heated to 466 to 482 °C (871 to 900 °F), quenched and aged at 121 °C (250 °F). T651 adds stretching to relieve quench stress in plate. Alcoa’s note on the ASM sheet states that the T7351 temper improves resistance to stress-corrosion cracking. Its strength is lower than T6, and the T6 sheet does not print it.

Heat and Weight

The alloy conducts 130 W/m·K (75.1 Btu/hr·ft·°F), 22 % less than 6061-T6. Its melting range starts at 477 °C (890 °F). Its ratio of strength to density is about 204, close to 224 for Ti-6Al-4V, in MPa per g/cm³.

ISO 286 IT Grades for Machined Holes and Shafts

An IT grade fixes the width of a size tolerance by nominal size, and temperature can use up most of the band before a part is measured.

What an IT Grade StatesISO 286 defines international tolerance grades for nominal sizes up to 3.15 m. A grade is a number prefixed with IT, from IT01 and IT0 through IT1 to IT18, and as the grade number rises the tolerance rises with it, and for a larger nominal size at the same grade it rises again.

Machining Ti-6Al-4V Grade 5 Titanium

Titanium cuts slowly because it holds heat at the tool and flexes under load, and its condition and cleanliness after the cut matter as much as the cutting data.

Ti-6Al-4V Grade 5 as a Machined MaterialGrade 5 is a two-phase alpha plus beta titanium alloy, with aluminum as the alpha stabilizer and vanadium as the beta stabilizer, and ATI calls it the most widely used titanium grade. The ASTM B348 composition limits for bar, printed by voestalpine, are 5.50 to 6.75 % aluminum, 3.50 to 4.50 % vanadium, 0.20 % oxygen at most, 0.40 % iron at most, 0.08 % carbon at most, 0.05 % nitrogen at most, 0.015 % hydrogen at most, and 0.10 % for any other element, 0.40 % in total.

Request a Metal CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Metal CNC chosen.

Request a Quote