Ultimate Tensile Strength

Ultimate tensile strength is the highest stress a metal carries in a tensile test, quoted in MPa or ksi.

Every Ultimate Tensile Strength article of the Metal CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Ultimate tensile strength is the highest stress a metal carries in a tensile test, quoted in MPa or ksi. It is the headline figure of most data sheets. Strength belongs to the alloy and its temper or condition, and it falls as temperature rises.

Aluminum

ASM gives 6061-T6 a typical ultimate tensile strength of 310 MPa (45,000 psi) and 7075-T6 one of 572 MPa (83,000 psi). The ratio is about 1.8, while the modulus differs by only 4 %. Strength therefore nearly doubles without making a part much stiffer.
Read More

Stainless at Temperature

ASTM A240 sets a minimum of 517 MPa (75 ksi) for 316 plate. Cleveland-Cliffs gives a typical 627 MPa (91 ksi) at room temperature for 316 sheet. The figure holds near 490 MPa (71.1 ksi) out to 427 °C (800 °F) and is 472 MPa (68.4 ksi) at 538 °C (1,000 °F). It falls to 350 MPa (50.7 ksi) at 649 °C (1,200 °F) and 212 MPa (30.7 ksi) at 760 °C (1,400 °F).

Titanium

Voestalpine gives annealed Grade 5 900 to 1070 MPa (131 to 155 ksi). Voestalpine gives 900 to 1070 MPa (131 to 155 ksi) annealed. ASM’s ELI print gives 860 MPa (125 ksi) for Grade 23.

Ratio to Density

Divided by density, ultimate tensile strength gives about 224 for Ti-6Al-4V, 204 for 7075-T6 and 115 for 6061-T6, in MPa per g/cm³. The A240 minimum of 316 gives 64 on the same basis. Titanium and 7075 come close, and they separate on temperature range, corrosion behavior and difficulty of cutting.

Machining Ti-6Al-4V Grade 5 Titanium

Titanium cuts slowly because it holds heat at the tool and flexes under load, and its condition and cleanliness after the cut matter as much as the cutting data.

Ti-6Al-4V Grade 5 as a Machined MaterialGrade 5 is a two-phase alpha plus beta titanium alloy, with aluminum as the alpha stabilizer and vanadium as the beta stabilizer, and ATI calls it the most widely used titanium grade. The ASTM B348 composition limits for bar, printed by voestalpine, are 5.50 to 6.75 % aluminum, 3.50 to 4.50 % vanadium, 0.20 % oxygen at most, 0.40 % iron at most, 0.08 % carbon at most, 0.05 % nitrogen at most, 0.015 % hydrogen at most, and 0.10 % for any other element, 0.40 % in total.

Machining 303 and 316 Stainless Steel

Stainless grade choice for a machined part is a trade between how freely it cuts and how well it resists the environment it works in.

Choosing 303 or 316 for a Machined Stainless PartThe choice sits on one trade. 303 is the free-machining modification of the basic 18 % chromium, 8 % nickel stainless, and it is produced to cut well.

Request a Metal CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Metal CNC chosen.

Request a Quote