Hardness

Hardness is a metal's resistance to indentation, read on a scale such as Brinell or Rockwell, and it tracks strength and tool wear.

Every Hardness article of the Metal CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Hardness is a metal’s resistance to indentation, read on a scale such as Brinell or Rockwell, and it tracks strength and tool wear. A harder alloy dulls a cutting edge faster on a long cut. Within one alloy, heat treatment moves hardness, and with it the size of the burr the part leaves.

Figures by Metal

ASM gives 6061-T6 a Brinell hardness of 95 and 7075-T6 one of 150. Both were read with a 500 g (1.1 lb) load on a 10 mm (0.39 in.) ball. Carpenter gives annealed 303 about 160 Brinell. ASTM A240 limits 316 plate to 217 Brinell at most. ATI gives Ti-6Al-4V Rockwell C 30 to 34 annealed and about 35 to 39 when aged.
Read More

Effect of Heat Treatment

Voestalpine prints about 330 HV for annealed Grade 5 bar. Aging at 524 to 552 °C (975 to 1,025 °F) raises strength and hardness by about 20 %, to 360 BHN. Carpenter notes that 303 gains strength and hardness when cold worked. A tool that rubs instead of cutting therefore hardens the surface it is about to remove.

Effect on Burrs

In the A356 case study of the burr review, the peak-aged condition reached 85 to 90 HRE. It gave the smallest burrs of the five conditions. The review’s explanation is that a harder matrix resists deformation, so the metal shears instead of folding over the edge. The smallest burr came with the highest cutting force. The silicon particles of the alloy also abrade the tool edge, the review adds.

Certificates and Documents That Ship With a Machined Metal Lot

Each document proves something different, so the order names the certificate type, the traceability, the process reports and the inspection data it expects.

The Documents That Travel With a Machined Metal LotA lot of machined metal parts usually travels with four kinds of paper, each issued by a different party and each proving something different. Confusing them is the most common reason a file looks complete and is not.

Thread Milling and Tapping Internal Threads in Metal Step by Step

An internal thread is decided at the drill, so gauge the minor diameter, size the drill to the engagement, then tap or mill with the entry and feed checked.

Tapping or Thread Milling for an Internal ThreadBoth methods start from the same drilled hole and end at the same gauge, and they differ in how the thread form gets into the wall. A tap cuts or forms the whole thread in one axial stroke, its size fixed by the tool.

Roughing and Finishing Passes in CNC Milling From Stock to Final Size

Rough to an even allowance, program the feed for the chip each pass really makes, and finish with a small constant depth so size depends on the tool, not the stock.

Roughing to Finishing in Milling, Pass by PassA milled part rarely reaches its size in one cut. The material is removed in stages, each with its own job, its own tool and its own engagement, and each leaves the next a predictable amount of stock.

Machining C36000 Free-Cutting Brass for Turned Parts

C36000 cuts so freely that spindle speed, chip control and finish usually set the cycle, so name the temper, the specification and any later joining on the order.

What Makes C36000 the Reference Brass for Turned PartsC36000 is a leaded copper-zinc alloy built to be cut. The Copper Development Association's data page gives its composition as 60.0 to 63.0 % copper, 2.5 to 3.0 % lead, iron at 0.35 % maximum and zinc as the remainder, with copper plus the named elements at 99.5 % minimum.

Machining 1045 and 4140 Carbon and Alloy Steel

The hardness and condition on the bar certificate set the speed, depth of cut and power for 1045 and 4140, so put the range on the order.

How 1045 and 4140 Differ Before the First CutThe two grades share a carbon level and little else. FM Carbide's technical reference gives 1045 as a plain medium-carbon steel of 0.43 to 0.50 % carbon and 0.60 to 0.90 % manganese, with phosphorus at 0.04 % and sulfur at 0.05 % maximum, and no deliberate chromium, molybdenum or nickel.

How Burrs Form on Machined Aluminum and How They Come Off

A burr is the last chip, so its size follows the alloy, the temper and the tool, and a signed edge size on the drawing turns it into a measurement.

Why a Cutting Tool Leaves a Burr on AluminumA burr is a projection of material beyond the workpiece limits. Its opposite is a negative burr, a missing portion of the edge where material broke away instead of being pushed.

Machining Ti-6Al-4V Grade 5 Titanium

Titanium cuts slowly because it holds heat at the tool and flexes under load, and its condition and cleanliness after the cut matter as much as the cutting data.

Ti-6Al-4V Grade 5 as a Machined MaterialGrade 5 is a two-phase alpha plus beta titanium alloy, with aluminum as the alpha stabilizer and vanadium as the beta stabilizer, and ATI calls it the most widely used titanium grade. The ASTM B348 composition limits for bar, printed by voestalpine, are 5.50 to 6.75 % aluminum, 3.50 to 4.50 % vanadium, 0.20 % oxygen at most, 0.40 % iron at most, 0.08 % carbon at most, 0.05 % nitrogen at most, 0.015 % hydrogen at most, and 0.10 % for any other element, 0.40 % in total.

Machining 303 and 316 Stainless Steel

Stainless grade choice for a machined part is a trade between how freely it cuts and how well it resists the environment it works in.

Choosing 303 or 316 for a Machined Stainless PartThe choice sits on one trade. 303 is the free-machining modification of the basic 18 % chromium, 8 % nickel stainless, and it is produced to cut well.

Request a Metal CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Metal CNC chosen.