Fatigue

Fatigue is the weakening of a part under repeated loads, and fatigue strength is the stress it survives for a stated number of cycles.

Every Fatigue article of the Metal CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Fatigue is the weakening of a part under repeated loads, and fatigue strength is the stress it survives for a stated number of cycles. ASM’s aluminum sheets state it at 500 million completely reversed cycles. Coatings and finishing steps can lower it, so the whole process sequence of a cyclically loaded part matters.

Aluminum Figures

ASM gives 6061-T6 a fatigue strength of 96.5 MPa (14,000 psi) and 7075-T6 one of 159 MPa (23,000 psi). That gap decides most structural cases between the two alloys. For titanium, ATI lists a hotter mill anneal where high fatigue strength is wanted. That is a mill treatment, not one for a finished part. The 7075 figure runs about 1.6 times higher on fatigue strength, as it does on hardness.
Read More

Effect of Coatings

MIL-A-8625 states that anodic coatings can severely reduce the fatigue properties of aluminum alloys. The loss grows with coating thickness, as a general rule. Types I and IB are used on fatigue-critical components because their coatings are thin. Types IC and IIB carry maximum coating weights for the same reason. If a higher IIB weight is acceptable, the document says to specify Type II instead. A part that is both cyclically loaded and hard coated has two requirements that pull against each other.

Effect of Deburring

The burr review lists effects on fatigue life among the side effects of brush deburring. Bonded abrasives also affect residual stress and surface quality. A finishing step chosen for the edge can therefore reach the fatigue life of the part.

How Burrs Form on Machined Aluminum and How They Come Off

A burr is the last chip, so its size follows the alloy, the temper and the tool, and a signed edge size on the drawing turns it into a measurement.

Why a Cutting Tool Leaves a Burr on AluminumA burr is a projection of material beyond the workpiece limits. Its opposite is a negative burr, a missing portion of the edge where material broke away instead of being pushed.

MIL-A-8625 Anodizing Types and Classes for Machined Aluminum

MIL-A-8625 names the bath, color state, weight or thickness and sealing of an anodized coating, and each choice moves the size of a machined part.

What MIL-A-8625 Covers and What the Types MeanRevision F covers six types and two classes of electrolytically formed anodic coatings on aluminum and aluminum alloys for non-architectural uses. The types differ by the bath and the weight of the coating: Type I is conventional chromic acid anodizing, Type IB a low-voltage chromic acid process, Type IC a non-chromic acid process offered as a non-chromate alternative, Type II conventional sulfuric acid anodizing, Type IIB a thin sulfuric acid process that is also a non-chromate alternative, and Type III the hard anodic coating.

Request a Metal CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Metal CNC chosen.

Request a Quote