Composition Limits

Composition limits are the minimum and maximum percentages of each element that an alloy's specification allows.

Every Composition Limits article of the Metal CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Composition limits are the minimum and maximum percentages of each element that an alloy’s specification allows. They define the alloy more firmly than any property figure. A mill certificate reports the actual analysis against them. A few tenths of a percent of one element can change how a metal cuts, corrodes or takes a coating.

Aluminum Alloys

The Aluminum Association limits on ASM’s sheets give 6061 0.8 to 1.2 % magnesium and 0.4 to 0.8 % silicon. They give 7075 5.1 to 6.1 % zinc, 2.1 to 2.9 % magnesium and 1.2 to 2.0 % copper. MIL-A-8625 does not apply Type I or Type III, unless the contract says so, to alloys above 5 % nominal copper. Type III is not applied above 8 % nominal silicon without approval.
Read More

Stainless Grades

Ugitech gives 303 17 to 19 % chromium, 8 to 10 % nickel and at least 0.15 % sulfur. Grade 316 carries 16 to 18 % chromium, 10 to 14 % nickel and 2 to 3 % molybdenum. Its sulfur is held to 0.03 % at most. The sulfur limit of 303 is five times that of 316, and molybdenum is the reverse. Those two rows decide between cutting behavior and corrosion behavior.

Titanium Grades

ASTM B348 limits Grade 5 bar to 5.50 to 6.75 % aluminum and 3.50 to 4.50 % vanadium. Oxygen is held to 0.20 %, iron to 0.40 %, carbon to 0.08 %, nitrogen to 0.05 % and hydrogen to 0.015 %. Grade 23 ELI lowers oxygen to 0.13 %, for better ductility and toughness at some cost in strength. The interstitial elements are the ones that move when a part is heated in air.

Machining Ti-6Al-4V Grade 5 Titanium

Titanium cuts slowly because it holds heat at the tool and flexes under load, and its condition and cleanliness after the cut matter as much as the cutting data.

Ti-6Al-4V Grade 5 as a Machined MaterialGrade 5 is a two-phase alpha plus beta titanium alloy, with aluminum as the alpha stabilizer and vanadium as the beta stabilizer, and ATI calls it the most widely used titanium grade. The ASTM B348 composition limits for bar, printed by voestalpine, are 5.50 to 6.75 % aluminum, 3.50 to 4.50 % vanadium, 0.20 % oxygen at most, 0.40 % iron at most, 0.08 % carbon at most, 0.05 % nitrogen at most, 0.015 % hydrogen at most, and 0.10 % for any other element, 0.40 % in total.

Machining 303 and 316 Stainless Steel

Stainless grade choice for a machined part is a trade between how freely it cuts and how well it resists the environment it works in.

Choosing 303 or 316 for a Machined Stainless PartThe choice sits on one trade. 303 is the free-machining modification of the basic 18 % chromium, 8 % nickel stainless, and it is produced to cut well.

Request a Metal CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Metal CNC chosen.

Request a Quote