Finishing Pass

A finishing pass is the last cut on a surface, taken with a small and constant depth to bring it to size and finish.

Every Finishing Pass article of the Metal CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A finishing pass is the last cut on a surface, taken with a small and constant depth to bring it to size and finish. It follows roughing and usually semi-finishing, which leave it an even allowance so that the tool deflects by the same amount everywhere.

Depth and Feed

The finishing pass is light. Cutting Tool Engineering’s tables for medium-carbon steel give a finishing turning pass of 1.0 mm (0.040 in.) at 0.18 mm (0.007 in.) per revolution, against 7.6 mm (0.300 in.) and 0.51 mm (0.020 in.) for roughing. For hard milling, a Modern Machine Shop report gives finishing depths of 0.10 to 0.51 mm (0.004 to 0.020 in.). With a 0.8 mm nose radius, the finishing feed above leaves a theoretical peak-to-valley height of about 5 µm (200 µin.), against about 41 µm for the roughing feed.
Read More

Even Allowance

A finishing tool that meets an uneven allowance cuts deeper in some places than others and leaves the size varying with the stock it finds. A semi-finishing or rest-milling pass removes the steps a larger roughing tool leaves in corners, and ISCAR notes that smaller allowances call for more accurate tools, such as solid end mills with good axial symmetry. Autodesk’s thread milling operation offers a repeat of the final finishing pass to remove stock left by tool deflection.

Tool and Heat

Finishing calls for sharper geometries and fine-grained substrates. Its small chips carry less heat away, which is why coolant matters most in this pass, and switching coolant off and on to inspect the part can halve tool life.

Thermal Effect

On a machine that has been idle, a finishing pass taken first carries the cold machine’s error into the part, so the machine is warmed before the pass that sets size.

Behavior

A finishing pass on a tight surface specification is the cut least likely to behave as a catalogue says, because wear grooves at fine feeds, flank wear and built-up edge all move the real finish away from the theoretical one.

Cycle Time of a Machined Part From Program to Time per Part

Time per part is cutting, moving, changing and handling plus the lot's share of setup, so check what a quoted cycle time includes before comparing.

What Makes Up the Cycle Time of a Machined PartA CNC program's time has three machine components. Autodesk's help for the machining time tool in its CAM software defines the estimate as the sum of feed time, the time for non-cutting traverse moves at the machine's fastest rate, and tool-change time, and it reports each with its distance and the number of tool changes.

Roughing and Finishing Passes in CNC Milling From Stock to Final Size

Rough to an even allowance, program the feed for the chip each pass really makes, and finish with a small constant depth so size depends on the tool, not the stock.

Roughing to Finishing in Milling, Pass by PassA milled part rarely reaches its size in one cut. The material is removed in stages, each with its own job, its own tool and its own engagement, and each leaves the next a predictable amount of stock.

Surface Roughness Ra by Machining Operation From Roughing to Grinding

The feed and nose radius of the last pass set the finish, so pick the process from the Ra band and measure with the cutoff the profile calls for.

Typical Ra From Turning, Milling and GrindingEach process leaves its own range. Keyence, a maker of roughness and profile instruments, publishes typical Ra values for finishing operations and stresses that real results depend on material, tooling and parameters.

Machining 1045 and 4140 Carbon and Alloy Steel

The hardness and condition on the bar certificate set the speed, depth of cut and power for 1045 and 4140, so put the range on the order.

How 1045 and 4140 Differ Before the First CutThe two grades share a carbon level and little else. FM Carbide's technical reference gives 1045 as a plain medium-carbon steel of 0.43 to 0.50 % carbon and 0.60 to 0.90 % manganese, with phosphorus at 0.04 % and sulfur at 0.05 % maximum, and no deliberate chromium, molybdenum or nickel.

How Many Parts One Cutting Edge Makes in a Machined Run

The parts an edge makes equal its minutes of life divided by the minutes each part spends on it, so a faster cycle can use more edges than it saves.

What Decides How Many Parts a Cutting Edge Can MakeParts per edge is a quotient. The numerator is the tool life, the minutes a cutting edge can stay in contact with the workpiece before it reaches the wear criterion.

Machining Center Thermal Drift and the Accuracy of the First Part

A ball screw grows with the heat of the work itself, so warm the machine at the production feed and check the datum before the first part counts.

Why a Cold Machine Cuts a Different Size Than a Warm OneA feed axis converts motor rotation to slide motion through a recirculating ball screw. When the control closes its position loop through a rotary encoder on the motor, the controlled quantity is the motor rotor position, and the slide position is inferred from the screw pitch.

Request a Metal CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Metal CNC chosen.

Request a Quote