Meaning
The alloy 6061-T6 is a 6000 series aluminum alloy of magnesium and silicon, heat treated and artificially aged to the T6 temper. The Aluminum Association limits printed on ASM’s sheet are 0.8 to 1.2 % magnesium and 0.4 to 0.8 % silicon. Beside 7075-T6, it is the lower-strength and more ductile of the two aluminum alloys most machined. ASM lists camera lens mounts, couplings, marine fittings, valve parts and hinge pins among its uses.Datasheet Figures
ASM prints a typical ultimate tensile strength of 310 MPa (45,000 psi) and a yield strength of 276 MPa (40,000 psi). Elongation is 12 % in 1.6 mm (1/16 in.) sheet and 17 % in 12.7 mm (1/2 in.) bar. Brinell hardness is 95, and fatigue strength at 500 million cycles is 96.5 MPa (14,000 psi). The modulus is 68.9 GPa (10,000 ksi) and the density 2.70 g/cm³ (0.0975 lb/in³). These are Aluminum Association typical values, labeled not for design.Read More
Joint Figures
The 6061 sheet carries three rows that the 7075 sheet lacks. Ultimate bearing strength is 607 MPa (88,000 psi) and bearing yield strength 386 MPa (56,000 psi), at an edge distance of twice the pin diameter. Notched tensile strength is 324 MPa (47,000 psi). A pinned or bolted joint reads these rows first.Burr Behavior
In drilling tests reviewed for these resources, 6061-T6 produced both uniform burrs and the crown burrs that are hard to remove. The alloy 6262-T6, which is 6061 with 0.5 % lead and 0.4 % bismuth, produced only uniform burrs. ASM adds that the T8 and T9 tempers of 6061 give better chipping than T6. Chip form is a machining property that the machinability rating of 50 cannot express.Dimensional Behavior
The alloy expands 23.6 µm/m·°C (13.1 µin/in·°F). A 25 mm (0.98 in.) feature that warms by 20 °C (36 °F) uses 91 % of its IT6 band. Its conductivity of 167 W/m·K (96.5 Btu/hr·ft·°F) sheds heat 28 % faster than 7075-T6. A plate 3 mm (0.12 in.) thick on supports 300 mm (11.8 in.) apart sags 54 µm (0.0021 in.) under its own weight.