Roughing

Roughing is the first, heavy stage of cutting that removes most of the stock and leaves a margin for the finishing passes.

Every Roughing article of the Metal CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Roughing is the first, heavy stage of cutting that removes most of the stock and leaves a margin for the finishing passes. It loads the machine, the tool and the part far more than finishing does. What roughing releases or heats can move the surfaces that finishing cuts later.

Heat Load

HEIDENHAIN gives typical roughing feeds of 3 to 4 m/min (9.8 to 13.1 ft/min). Finishing runs at 0.5 to 1 m/min (1.6 to 3.3 ft/min). Axes move under cutting load more than 80 % of the time in roughing and less than 10 % in finishing. Roughing therefore heats the ball screws, and finishing lets them cool. A part finished after a long roughing cycle is cut on a warmer machine than one finished first.
Read More

Stress Sequence

For a thin or flat part, a common sequence is to rough it, relieve it and then finish it. For titanium, ATI prints a stress relief of 538 to 649 °C (1,000 to 1,200 °F) for 1 to 8 hours. The stress released by roughing then cannot move the finished face. The data sheets do not prescribe that order, so the drawing or the process plan names it.

Tool Wear Limit

Roughing tools reach their wear limit on the heavy cuts. The Lund study notes that tool life models fitted on roughing data fit poorly when carried into finishing on stainless steel. There the thin chip cuts into a surface the previous pass hardened. Finishing tools reach their limit where a small wear width already changes the size and surface of the part.

Cycle Time of a Machined Part From Program to Time per Part

Time per part is cutting, moving, changing and handling plus the lot's share of setup, so check what a quoted cycle time includes before comparing.

What Makes Up the Cycle Time of a Machined PartA CNC program's time has three machine components. Autodesk's help for the machining time tool in its CAM software defines the estimate as the sum of feed time, the time for non-cutting traverse moves at the machine's fastest rate, and tool-change time, and it reports each with its distance and the number of tool changes.

Thread Milling and Tapping Internal Threads in Metal Step by Step

An internal thread is decided at the drill, so gauge the minor diameter, size the drill to the engagement, then tap or mill with the entry and feed checked.

Tapping or Thread Milling for an Internal ThreadBoth methods start from the same drilled hole and end at the same gauge, and they differ in how the thread form gets into the wall. A tap cuts or forms the whole thread in one axial stroke, its size fixed by the tool.

Roughing and Finishing Passes in CNC Milling From Stock to Final Size

Rough to an even allowance, program the feed for the chip each pass really makes, and finish with a small constant depth so size depends on the tool, not the stock.

Roughing to Finishing in Milling, Pass by PassA milled part rarely reaches its size in one cut. The material is removed in stages, each with its own job, its own tool and its own engagement, and each leaves the next a predictable amount of stock.

Surface Roughness Ra by Machining Operation From Roughing to Grinding

The feed and nose radius of the last pass set the finish, so pick the process from the Ra band and measure with the cutoff the profile calls for.

Typical Ra From Turning, Milling and GrindingEach process leaves its own range. Keyence, a maker of roughness and profile instruments, publishes typical Ra values for finishing operations and stresses that real results depend on material, tooling and parameters.

Machining 1045 and 4140 Carbon and Alloy Steel

The hardness and condition on the bar certificate set the speed, depth of cut and power for 1045 and 4140, so put the range on the order.

How 1045 and 4140 Differ Before the First CutThe two grades share a carbon level and little else. FM Carbide's technical reference gives 1045 as a plain medium-carbon steel of 0.43 to 0.50 % carbon and 0.60 to 0.90 % manganese, with phosphorus at 0.04 % and sulfur at 0.05 % maximum, and no deliberate chromium, molybdenum or nickel.

How Many Parts One Cutting Edge Makes in a Machined Run

The parts an edge makes equal its minutes of life divided by the minutes each part spends on it, so a faster cycle can use more edges than it saves.

What Decides How Many Parts a Cutting Edge Can MakeParts per edge is a quotient. The numerator is the tool life, the minutes a cutting edge can stay in contact with the workpiece before it reaches the wear criterion.

Machining Center Thermal Drift and the Accuracy of the First Part

A ball screw grows with the heat of the work itself, so warm the machine at the production feed and check the datum before the first part counts.

Why a Cold Machine Cuts a Different Size Than a Warm OneA feed axis converts motor rotation to slide motion through a recirculating ball screw. When the control closes its position loop through a rotary encoder on the motor, the controlled quantity is the motor rotor position, and the slide position is inferred from the screw pitch.

Flatness of Machined Metal Plates

A plate's measured flatness depends on the stress in its stock, its temperature and its support, as well as on the cut that finished it.

What Flatness General Tolerances AllowA machined plate leaves the mill with faces cut flat. Where the drawing gives a face no flatness of its own, ISO 2768-2 sets the tolerance it is held to.

Machining Ti-6Al-4V Grade 5 Titanium

Titanium cuts slowly because it holds heat at the tool and flexes under load, and its condition and cleanliness after the cut matter as much as the cutting data.

Ti-6Al-4V Grade 5 as a Machined MaterialGrade 5 is a two-phase alpha plus beta titanium alloy, with aluminum as the alpha stabilizer and vanadium as the beta stabilizer, and ATI calls it the most widely used titanium grade. The ASTM B348 composition limits for bar, printed by voestalpine, are 5.50 to 6.75 % aluminum, 3.50 to 4.50 % vanadium, 0.20 % oxygen at most, 0.40 % iron at most, 0.08 % carbon at most, 0.05 % nitrogen at most, 0.015 % hydrogen at most, and 0.10 % for any other element, 0.40 % in total.

Request a Metal CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Metal CNC chosen.

Request a Quote